The SmartPrep™ is a flowing-gas degassing unit which removes adsorbed contaminants from the surface and pores of your sample in preparation for analysis. It contains six sample ports, each one independently temperature-controlled for greater flexibility. It contains two serial ports, one for connecting to the computer and the other available for connection of an additional SmartPrep. The temperature, ramp rates, and soak times of each sample are individually controlled by computer. Up to five ramps and soaks are allowed. All degas information is integrated into the sample data file for easy reference in the future. The SmartPrep is the recommended degassing unit for the TriStar; however, you may furnish your own degassing method if desired, or use the Micromeritics FlowPrep™ or VacPrep™.
Specifications
|
Degas Method:
|
Flowing Gas
|
|
Number of stations:
|
6
|
| Sample tubes |
Up to 30mm OD. (1.18 in.) |
| Temperature Range: |
Ambient to 425° C, in 1° C increments; each station is controlled separately |
|
Accuracy:
|
0-100° C : ±5° C 100-300° C : ±10° C 300-425° C : ±15° C
|
| Soak Time: |
0 to 999 minutes, in one-minute increments (Five ramp and soaks are allowed)
|
|
Cooling Time:
|
From 425° C to 60° C in less than 60 minutes
|
| Physical |
Height: 43 cm (17 in.) Width: 42 cm (16.5 in.) Depth: 30.5 cm (12 in.) Weight: 15 Kg (33 lbs)
|
| Power |
500 VA |
|
Miscellaneous:
|
ISO 9001 manufacturer CE certified |