ASTM B330-12 Standard Test Method for Fisher Number of Metal Powders and Related Compounds – Committee B09 on Metal Powders and Metal Powder Products

ASTM B761-06(2011) Standard Test Method for Particle Size Distribution of Metal Powders and Related Compounds by X-Ray Monitoring of Gravity Sedimentation – Committee B09 on Metal Powders and Metal Powder Products

ASTM B822-10 Standard Test Method for Particle Size Distribution of Metal Powders and Related Compounds by Light Scattering – Committee B09 on Metal Powders and Metal Powder Products

ASTM C110-11 Standard Test Methods for Physical Testing of Quicklime, Hydrated Lime and Limestone – Committee C07 on Lime

ASTM C690-09 Standard Test Method for Particle Size Distribution of Alumina or Quartz Powders by Electrical Sensing Zone Technique – Committee C21 on Whitewares and Related Products

ASTM C958-92(2007) Standard Test Method for Particle Size of Alumina or Quartz by X-Ray Monitoring of Gravity Sedimentation – Committee C21 on Whitewares and Related Products

ASTM C1070-01(2007) Standard Test Method for Determining Particle Size Distribution of Alumina or Quartz by Laser Light Scattering – Committee C28 on Advanced Ceramics

ASTM D4438-85(2007) Standard Test Method for Particle Size Distribution of Catalytic Material by Electronic Counting – Committee D32 on Catalysts

ASTM D4464-10 Standard Test Method for Particle Size of Catalytic Materials by Laser Light Scattering – Committee D32 on Catalysts

ASTM D5861-07 Standard Guide for Significance of Particle Size Measurements of Coating Powders – Committee D01 on Paint and Related Coatings, Materials  and Applications

ASTM E2490-09 Standard Guide for Measurement of Particle Size Distribution of Nanomaterials in Suspension by Photon Correlation Spectroscopy (PCS) – Committee E56 on Nanotechnology

ASTM F577-03(2009) Standard Test Method for Particle Size Measurement of Dry Toners – Committee F05 on Business Imaging Products

New Test Method for Particle Size Distribution of Advanced Ceramics by X-Ray Monitoring of Gravity Sedimentation – Committee C28 on Advanced Ceramics

ASTM F2149-01(2007) Standard Test Method for Automated Analysis of Cells – the Electrical Sensing Zone Method of Enumerating and Sizing Single Cell Suspensions – Committee F04 on Medical and Surgical Materials and Devices



ASTM Test Methods   

ASTM Test Methods appropriate for Micromeritics and Particulate Systems Instruments



Bibliography of Papers   

Approximately 10,000 peer reviewed papers in which one or more Micromeritics products are referenced.



DFT / NLDFT Density Functional Theory   

Facts about the development of DFT



FAQs   

A sortable database of Frequently Asked Questions





Glossary of Terms   

Glossary of Terms



Request for Information   

A form for personal replies to your questions and inquiries.