Smart VacPrep
Smart VacPrep is an advanced six-port system that utilizes vacuum to prepare samples by heating and evacuation.
![smart prep 2 Smart VacPrep Gas Adsorption Sample Preparation Device](https://www.micromeritics.com/wp-content/uploads/smart-prep-2.jpg)
Specifications
Capacity: Six ports
Degas Method: Heat and vacuum
Vacuum Control: Servo-controlled rates to minimize or eliminate sample elutriation
Evacuation Rate: Selectable evacuation rate from 1.0 to 50.0 mmHg/s
Heating of Samples: Heating mantles
Temperature Range: 40 to 450 ºC in one degree increments
Temperature Control: One ramp during evacuation phase, five additional ramps during subsequent phases
Temperature Accuracy: Deviation less than ±10 ºC at the sensing thermocouple embedded in the heating mantle
Heating Ramp Rate: Selectable from 0.1 ºC per minute to 10 ºC per minute
Hold Time: Zero to 999 minutes in one-minute increments
Backfill Options: Automatic backfill
Dimensions: Height 69 cm (27 in.), Width 53 cm (21 in.), Depth 43 cm (17 in.)
Weight: 70 lbs (32 kg)